泰鋼煉鋼廠積極開展工藝優(yōu)化課題攻關
發(fā)布時間:2014-11-24 10:11
編輯:GC201
來源:互聯(lián)網(wǎng)
60
.TRS_Editor TABLE{font-family:宋體;font-size:14px;}.TRS_Editor{font-family:宋體;font-size:14px;}.TRS_Editor P{font-family:宋體;font-size:14px;margin-top:0;margin-bottom:0;line-height:1.4;}.TRS_Editor H1,.TRS_Editor H2,.TRS_Editor H3,.TRS_Editor H4,.TRS_Editor H5,.TRS_Editor H6,.TRS_Editor HR,.TRS_Editor BLOCKQUOTE,.TRS_Editor DL,.TRS_Editor DD,.TRS_Editor DT,.TRS_Editor OL,.TRS_Editor UL,.TRS_Editor LI,.TRS_Editor PRE,.TRS_Editor CODE,.TRS_Editor textarea,.TRS_Editor SELECT,.TRS_Editor CITE,.TRS_Editor PRE,.TRS_Editor CENTER,.TRS_Editor TABLE,.TRS_Editor DIV{margin-top:0;margin-bottom:0;line-height:1.4;}.TRS_Editor FORM,.TRS_Editor FIELDSET,.TRS_Editor LEGEND,.TRS_Editor SELECT,.TRS_Editor TR,.TRS_Editor TD,.TRS_Editor TH{margin-top:0;margin-bottom:0;line-height:1.4;}.TRS_Editor BUTTON,.TRS_Editor OPTION,.TRS_Editor ADDRESS,.TRS_Editor DFN,.TRS_Editor EM,.TRS_Editor VAR,.TRS_Editor KBD,.TRS_Editor INPUT,.TRS_Editor SMALL,.TRS_Editor SAMP,.TRS_Editor SUB,.TRS_Editor SUP,.TRS_Editor SPAN,.TRS_Editor A,.TRS_Editor B,.TRS_Editor I,.TRS_Editor U,.TRS_Editor S,.TRS_Editor STRONG,.TRS_Editor LABEL,.TRS_Editor IMG,.TRS_Editor BR,.TRS_Editor FONT{margin-top:0;margin-bottom:0;text-indent:0;} 本報訊 10月份以來,泰鋼集團煉鋼廠圍繞提高產(chǎn)品質(zhì)量、工藝改進、挖潛降耗等方面,開展了有效控制鋼水成分、提高連鑄坯表面質(zhì)量和設備精度等專項技術攻關。
為了有效提高鑄坯質(zhì)量,該廠先后邀請科研院校專家到現(xiàn)場進行論證和指導,根據(jù)專家的意見和建議,分別對結晶器水冷卻噴淋系統(tǒng)進行優(yōu)化;改變了二冷動態(tài)配水的方案,針對不同鋼種選擇不同的冷卻方法,基本解決了低合金高強度鋼的邊部橫裂紋問題,改善了鑄坯表面質(zhì)量。
同時,該廠轉爐煉鋼爐前班減少“富貴料”、增加“貧民餐”,其中轉爐車間爐前以石灰石代替部分石灰,噸鋼石灰加入量由原來的50千克降至31千克,平均噸鋼降低成本6.84元,每月直接創(chuàng)效102.6萬元。一次除塵系統(tǒng)的風機轉子使用周期壽命為7天左右,運行周期短。對此,該廠在風機機殼增加轉子反沖洗裝置,通過對轉子的在線沖洗,使轉子表面掛灰在水的沖洗下剝離脫落,減少轉子掛灰量,并根據(jù)吹煉時間,調(diào)整沖洗時間,延長了轉子的使用壽命,每月可節(jié)約費用2.5萬元。 (田志杰)
備注:數(shù)據(jù)僅供參考,不作為投資依據(jù)。